1926.502(d)(4): D-Ring and Snaphook Proof Test
D-rings and snaphooks must be proof-tested to 3,600 pounds without cracking, breaking or permanent deformation.
Official text: 29 CFR 1926.502(d)(4)
(4) Dee-rings and snaphooks shall be proof-tested to a minimum tensile load of 3,600 pounds (16 kN) without cracking, breaking, or taking permanent deformation.
1 citationsSource: eCFR, text current as of 2026-10-15. Read all of 1926.502.
Free toolbox talk for this rule
A 5-minute crew talk on 1926.502(d)(4), plus alerts when this rule changes. Free.
Where and how often it was cited
OSHA interpretation letters
Related parts of this rule
- 1926.502(d) Personal fall arrest systems 2,011 citations
- 1926.502(d)(17) 560 citations
- 1926.502(d)(15) 507 citations
- 1926.502(d)(16) 326 citations
- 1926.502(d)(16)(iii) 277 citations
- 1926.502(d)(21) 136 citations
- 1926.502(d)(6) 128 citations
- 1926.502(d)(6)(i) 111 citations
- 1926.502(d)(15)(ii) 55 citations
- 1926.502(d)(11) 44 citations
- 1926.502(d)(8) 17 citations
- 1926.502(d)(1) 17 citations
Get your crew competent
Trainers on Black Belt Safety: Marc Harvey, Dana Reyes
Trainers and suppliers: feature your business on this rule for $25/month.
About this page
Official text from the eCFR. Citation and injury numbers from public U.S. Department of Labor enforcement and accident records, copied nightly; 3-year window; data as of 2026-10-18. Federal OSHA only; state-plan rules are not counted. Plain-language text is a summary, not legal advice; the official text controls. Black Belt Safety is not part of OSHA or the Department of Labor.